I've read in one of the articles dealing with Alclad2 lacquers that one was supposed to keep the first coat very light, let it dry and then apply the second, final coat after 10-15 minutes. Well, I don't know if I should call my first pass with the airbrush as very light, after all my control of the airbrush is still rather hamfisted. Still, I was quite pleased with myself once I was finished - first signs of very nice metallic look were clearly visibile. And those scratches and small spatter dropplets would surely be covered by the final coat.
Well... once I was done with the second, heavier coat, four facts became visible to me, and I don't mean metaforically; they were really visble. First and foremost, my polishing of the the primer left a lot to be desired and resulted in a very uneven finish of the metallic paint. Second, any scratches on primed surface are 'reproduced' on the metallic surface. Third, airbrush spatter dropplets will not be covered by the subsequent lacquer coats. Fourth, working with Alclad2 isn't as easy as they want to make you believe!
In vain hope that the rather unpleasing finish would be improved with additional coats of Alclad, I sprayed on both a third and fourth coat within 24 hours of each other. Parts of the airplane where the primer was properly smoothed took on a very pleasing aluminium shine, but those with a bit rougher initial finish remained grayish and less shiny. Additional coats had no effect on scratches and spatter spots. In a final desperate effort, I sprayed two light coats of Alclad gloss varnish, hoping that its uniform shine would even things out - that step helped a little in respect of overall finish, but I was still not very pleased with final result.
I admit that I was very tempted to take the easy way out, grab the Aluminium spraycan from Tamiya and spray it over the unsatisfactory Alclad. However, not knowing how the two paints would react with each other - after all, Alclad is a lacquer and God only knows what content of Tamiya's brush cans is really based on (I'm pretty sure though that it isn't a purely acrylic). More importantly though, the mishap with Alclad was an honest mistake and part of a learning process. So, better to keep the 70 percent satisfactory job for future reference and hopefully as bottom of measuring stick of future improvement.
Pictures below (in pairs) show the model after first, second and final coat with Alclad's gloss varnish on top.